A FTIR study of the metal-support interactions and hydrogen spillover on Pd/TiO2 and Ni/TiO2

Nickel and palladium dispersed on titania support were submitted to reductive treatment, under hydrogen, at 200 and 500 ºC. After the reductive thermal treatment the materials were exposed to carbon monoxide (10 Torr) and analyzed in the infrared region. The increasing of the electronic density in t...

Full description

Bibliographic Details
Authors: Faccin, Flavio, Guedes, Fabiana Flores, Benvenutti, Edilson Valmir, Moro, Celso Camilo
Format: article
Status:Published version
Publication Date:2002
Country:Brasil
Institution:Universidade Federal do Rio Grande do Sul (UFRGS)
Repository:Repositório Institucional da UFRGS
Language:English
OAI Identifier:oai:www.lume.ufrgs.br:10183/23132
Online Access:http://hdl.handle.net/10183/23132
Access Level:Open access
Keyword:Interação metal-suporte
Espectroscopia : Infravermelho
Monóxido de carbono
Metal-support
Infrared
Titania
Carbon monoxide
Hydrogen spillover
Palladium
Nickel
Description
Summary:Nickel and palladium dispersed on titania support were submitted to reductive treatment, under hydrogen, at 200 and 500 ºC. After the reductive thermal treatment the materials were exposed to carbon monoxide (10 Torr) and analyzed in the infrared region. The increasing of the electronic density in the metallic d subshell, produced by the reductive thermal treatment, was monitored by the infrared stretching band shift of carbon monoxide adsorbed and it was interpreted as a consequence of the metal-support interactions. The highest effect was observed for Pd/TiO2 system. From the FTIR spectra was also observed that the hydrogen spillover was stronger on Pd/TiO2 than Ni/TiO2 system.