Inorganofunctionalization of Ti(IV) and Zr(IV) on the MCM-41 Surface and its Interaction with a Mixed Valence Complex to use as Isoniazid Sensing

In this work, it describes the preparation of Titanium and Zirconium functionalized MCM-41 and subsequent chemical modification with nickel hexacyanoferrate. The obtained materials (MTiNiH and MZrNiH) were characterized by Fourier Transform Infrared Spectroscopy (FTIR), Scanning Electron Microscopy...

ver descrição completa

Detalhes bibliográficos
Autores: de Souza Magossi, Maiara [UNESP], Fernandes, Daniela Silvestrini [UNESP], dos Santos Franco, Fernanda [UNESP], dos Santos Felipe, Alexsandro [UNESP], de Vicente, Fábio Simões [UNESP], do Carmo, Devaney Ribeiro [UNESP]
Tipo de documento: artigo
Estado:Versão publicada
Data de publicação:2021
País:Brasil
Recursos:Universidade Estadual Paulista (UNESP)
Repositório:Repositório Institucional da UNESP
Idioma:inglês
OAI Identifier:oai:repositorio.unesp.br:11449/207767
Acesso em linha:http://dx.doi.org/10.1007/s10904-021-02025-x
http://hdl.handle.net/11449/207767
Access Level:Acceso aberto
Palavra-chave:Cyclic voltammetry
Isoniazid
Mesoporous silica
Nickel hexacyanoferrate
Descrição
Resumo:In this work, it describes the preparation of Titanium and Zirconium functionalized MCM-41 and subsequent chemical modification with nickel hexacyanoferrate. The obtained materials (MTiNiH and MZrNiH) were characterized by Fourier Transform Infrared Spectroscopy (FTIR), Scanning Electron Microscopy (SEM), X-ray Dispersive Energy Spectroscopy (EDS), Porosity and Surface Area and Voltammetry Cyclic (VC). The cyclic voltammogram of MTiNiH and MZrNiH modified graphite paste were sensitive to isoniazid concentrations. The MTiNiH modified graphite pulp electrode showed an analytical curve with a linear response of 2.0 × 10–5 to 5.0 × 10–4 mol L−1 and detection limit of 6.12 × 10–6 mol L−1 and MZrNiH modified electrode showed an analytical curve with a linear response of 3.0 × 10–5 to 3.0 × 10–4 mol L−1 and detection limit of 1.66 × 10–5 mol L−1. After catalytic electro-oxidation of isoniazid, a study of the main interferents was performed and the recovery of isoniazid in a synthetic urine sample was also evaluated. The MTiNiH and MZrNiH materials stand out for presenting good detection limit and recovery efficiency in real samples. Therefore, these materials can be considered is a strong candidate for the construction of electrochemical sensors for quick and easy detection of isoniazid.