Desenvolvimento de catalisadores para reforma e oxidação combinadas do metano

In this work, we studied the effects of the promoters of support (ZrO2, La2O3, CeO2, CeO2-ZrO2, CeO2-ZrO2-La2O3 and La2O3) in the nickel catalysts supported on γ-Al2O3 were studied. The supports were prepared by wet impregnation on γ- Al2O3 (Alfa Aesar) with 10% by weight of oxides...

Descripción completa

Detalles Bibliográficos
Autor: Silva, Tatiana de Freitas
Tipo de recurso: tesis de maestría
Estado:Versión publicada
Fecha de publicación:2009
País:Brasil
Institución:Universidade Federal de São Carlos (UFSCAR)
Repositorio:Repositório Institucional da UFSCAR
Idioma:portugués
OAI Identifier:oai:repositorio.ufscar.br:20.500.14289/4025
Acceso en línea:https://repositorio.ufscar.br/handle/20.500.14289/4025
Access Level:acceso abierto
Palabra clave:Catálise
Metano
Reforma - metano
Oxidação parcial do metano
ENGENHARIAS::ENGENHARIA QUIMICA
Descripción
Sumario:In this work, we studied the effects of the promoters of support (ZrO2, La2O3, CeO2, CeO2-ZrO2, CeO2-ZrO2-La2O3 and La2O3) in the nickel catalysts supported on γ-Al2O3 were studied. The supports were prepared by wet impregnation on γ- Al2O3 (Alfa Aesar) with 10% by weight of oxides of cerium, zirconium, lanthanum, ceria-zirconia, ceria-lanthanum and lanthanum-zirconium. The addition of nickel was performed by impregnation of the supports using an aqueous solution of Ni(NO3)2.6H2O (Fluka), followed by drying at 373 K for 24 hours and calcined in synthetic air (80 ml / min) at 823 K for 5 h. The samples were characterized by dispersive spectroscopy X-ray (EDX), analysis of BET, X-ray diffraction (XRD), temperature programmed reduction (TPR), temperature programmed Desorption (TPD), and temperature programmed oxidation (TPO). The catalysts were studied for steam reforming, partial oxidation and oxidative reforming of methane. For steam reforming, the catalysts that have two promoters and the catalyst NiLaAl presented the highest catalytic activities. In the partial oxidation the values of conversion of methane produced by different catalysts are similar. In the oxidative reforming the catalysts that have only one type of promoter and the catalyst NiCeLaAl, above 500 º C showed the best catalytic performance.